Industrial synthesis steps of acrylic sheet

Nov 11, 2020 Leave a message

The industrial synthesis steps of acrylic sheet are divided into 5 steps:


Pulping part: After adding quantitative initiators, plasticizers and mold release agents to the monomers, the slurry with a conversion rate of about 10 is prepared after five dissolutions: determine the production cycle and improve production efficiency. In the pre-polymerization reaction, the initiator is decomposed at high temperature, the induction period is shortened, the monomer is activated, and the chain is lengthened. Through stirring, heat exchange is accelerated, and more heat of polymerization is eliminated in a short time. In order to promote the increase of monomer viscosity, the gel effect comes earlier. The degradation method can increase the monomer viscosity and is convenient for operation. Reduce volume shrinkage during polymerization. The ratio of monomer is 0.94, and the ratio of finished plexiglass is 1.17~1.19. If the monomer is directly polymerized into an acrylic sheet in the mold, volume shrinkage of 19 and 22% can be achieved. Such a large shrinkage rate brings difficulties to mold manufacturing, pouring and polymerization processes. After stirring. The specific gravity is generally about 0.96 to 0.98, which can reduce the shrinkage during polymerization. When the viscosity of the slurry increases, the leakage loss after casting the mold can be reduced.


Mechanical mold part: In two clean and dry silica flat glass, fill the four sides with cellophane strips (or hoses), control the gap distance, adjust the thickness of the finished product, and fill it after clamping with a clamp.

Irrigation section: Through calculation and measurement, the slurry produced in the pulping section is poured into the mold made in the forming section, and the air in the gap is discharged, so that the slurry is covered and sealed by the template.

Assembly part: Put the finished feed liquid into the water tank (or drying room). If it is a degradable slurry in the mold, it should be induced at a higher temperature for a period of time, and then kept at a lower temperature for a longer time, until the polymer in the mold hardens and the temperature rises. If the mold is a prepolymerized material slurry, it can be kept at low temperature for a long time until the polymer in the mold hardens, then increase the temperature and heat treatment: after the polymerization is completed, the temperature drops below 40OC. Remove the mold, take out the required polymer, the production is called "wool sheet".